Rogers RO4003C PCB

RO4003C sits one step above RO4350B in the same Rogers RO4000 family, and the step is smaller than the price suggests on paper: the dielectric constant moves from 3.48 to 3.38 and the dissipation factor from 0.0037 to 0.0027 at 10 GHz. This page is about what those two numbers actually buy, because the decision is rarely obvious and the wrong answer costs either money or margin.

RO4003C in one paragraph

It is a woven-glass-reinforced hydrocarbon laminate with ceramic filler — the same chemistry as RO4350B, formulated for lower loss. It is not PTFE, so it drills, plates and laminates on standard FR-4 tooling, and it bonds to FR-4 in a hybrid stack. That combination is why it appears in filters, couplers, power dividers and phased-array feed networks where the loss budget is tight but the production volume still has to be built inside a normal PCB fabrication operation rather than at a PTFE specialist.

The two numbers that separate it from RO4350B

PropertyRO4350BRO4003CDifference
Dk @ 10 GHz3.48 ± 0.053.38 ± 0.05−2.9 %
Df @ 10 GHz0.00370.0027−27 %
Tg (TMA)> 280 °C> 280 °Csame
Water absorption~0.06 %~0.06 %same
ProcessFR-4 compatibleFR-4 compatiblesame

The asymmetry is the whole story. A 2.9 % change in Dk barely moves the layout: on a 50 Ω microstrip, the trace width changes by roughly 1.5 %. A 27 % change in Df changes the loss budget by 27 % on the dielectric component. So the upgrade buys loss, not density, and it does so without forcing a redesign.

What 0.001 of Df buys in decibels

Dielectric loss is proportional to frequency, Df and the square root of Dk. Working it out for both materials gives a figure that is easier to argue with than a percentage:

FrequencyRO4350B (dB/in)RO4003C (dB/in)Difference
1 GHz0.0160.0110.005
5 GHz0.0800.0570.022
10 GHz0.1600.1150.045
20 GHz0.3190.2290.090
28 GHz0.4470.3210.125

At 10 GHz the saving is about 0.045 dB per inch. On a two-inch trace that is 0.09 dB — below the repeatability of most bench measurements and certainly below the value of the price difference. On a ten-inch feed network it is 0.45 dB, and on twenty inches it is 0.9 dB. That is the range where the material choice starts to decide whether the link closes.

These figures cover dielectric loss only. Conductor loss — which depends on copper roughness and on the finish — is not included, and at 10 GHz on ½ oz copper it can be the larger of the two. A design that switches to RO4003C but keeps a standard-profile copper foil may recover much less than the table suggests. If the loss budget is genuinely tight, specify low-profile copper at the same time.

Dk 3.38 changes the layout less than people expect

Because the Dk difference is small, an existing RO4350B layout can usually move to RO4003C with a width adjustment rather than a re-route. Three consequences worth checking:

  • Impedance shifts up slightly at fixed geometry. A 50 Ω line on RO4350B becomes roughly 51 Ω on RO4003C unless the width is increased by about 1.5 %.
  • Electrical length shrinks by about 1.5 %, because propagation velocity rises with lower Dk. On a phase-critical network — a phased-array feed, a delay line — this matters more than the impedance shift.
  • Physical length for a given phase stays close, so filters built on RO4350B normally re-tune with small adjustments rather than a new topology.

If the design is already at the edge of the etch tolerance, the width change is not free: a 3 mil trace becomes 3.05 mil, which is below what any shop can hold. In that case the geometry stays and the impedance is accepted slightly high, or the stack thickness is adjusted instead.

Hybrid stacks: three materials on one board

The most common construction we build is not all-RO4003C. A typical six-layer board uses RO4003C on the RF layers, RO4350B on an adjacent layer where the loss requirement is looser, and FR-4 or high-Tg FR-4 for the digital and power layers. Three materials in one lamination is normal for us, but it has to be designed:

  1. Keep the prepreg compatible with both. The bonding layer between RO4003C and FR-4 is a different product from the one between RO4003C and RO4350B. Using one prepreg throughout is the usual cause of delamination after thermal cycling.
  2. Check the CTE stack-up, not each material. The plated barrel passes through all three. Its survival depends on the combined expansion, which is why we review the full stack before tooling rather than the RF layers alone.
  3. Fix one lamination cycle. A three-material stack has one window that satisfies all of them. It gets qualified once and then repeated — re-deriving it per order is how thickness drift starts.

For boards that also carry high current, the combination is a thick copper inner layer with an RO4003C RF section, which is common in amplifier and antenna feed hardware. Layer counts above eight with mixed materials follow multilayer rules, and the stack should be reviewed through DFM review before the panel is released.

Where RO4003C is specified

  • Filters and diplexers. Narrow-band filters are sensitive to both Dk tolerance and loss; RO4003C's tighter loss figure keeps insertion loss inside the mask without adding gain stages.
  • Couplers and power dividers. Long coupled sections accumulate loss, so the per-inch difference compounds.
  • Phased-array feed networks. Where the feed line runs tens of inches across the panel and every 0.1 dB counts against the array's sidelobe performance.
  • Low-noise receiver front ends. Loss ahead of the first amplifier goes straight into the noise figure, so the material is part of the RF budget rather than a packaging decision.
  • Test and measurement hardware. Where the board is inside the instrument's calibration path and its loss has to be known and stable.

Where the premium is not worth paying

If the longest high-frequency trace is under about three inches and the system has 3 dB of margin, RO4003C is buying margin the design does not need. The same applies where the loss is dominated by connectors, cable assemblies or the package rather than the board. In both cases RO4350B delivers the same result at a lower material cost, and on short runs the difference in unit price can exceed the difference in performance by a wide margin.

The reverse mistake is more expensive: staying on RO4350B through prototype, then discovering at 28 GHz that the feed network is 1.2 dB short. That is not a material problem at that point — it is a schedule problem. If the frequency is above 20 GHz and the feed is longer than a few inches, the loss arithmetic belongs in the design review, not in the second prototype.

Fabrication: same line, tighter window

ParameterCapability
Layer count2 – 24 layers
Finished thickness0.5 mm – 6.0 mm
Minimum trace / space3 mil / 3 mil on ½ oz copper
Minimum drill0.2 mm mechanical
Copper foilStandard or low-profile (HVLP) on request — affects loss at 10 GHz and above
Surface finishENIG, immersion silver, OSP
Impedance controlSingle-ended and differential, ±10 % typical

The processes are the same as any FR-4 job, which is the point of the RO4000 family. What differs is the tolerance stack: because the loss advantage is the reason for the material, the copper foil profile and the finish both have to be controlled, or the advantage is spent on the surface. We state the foil type on the traveller so it can be verified later.

Impedance coupons and the report

Every RF order carries an impedance coupon in the panel. The report states the target, the measured value, the test method used and the coupon location, because a number without a method is not evidence. TDR on a coupon and VNA on the finished trace give different figures, and the gap is wide enough to matter when the tolerance is ±10 %.

Where the customer's qualification requires it, we can also supply a micro-section of the plated through-hole and the dielectric thickness measurement at the coupon. Both are destructive, so they are sampled rather than applied to every board — the sampling plan is agreed at order entry rather than assumed. The PCBA testing page covers fixture building and program development where the board also needs functional test, and the test methods page sets out what each option catches.

Assembly notes

RO4003C assemblies run on the same line as any other board: high-speed SMT placement with SPI before reflow, automatic through-hole for connectors, and X-ray inspection for area-array devices. Three points differ from a standard FR-4 job:

  • The reflow profile follows the most sensitive material in a hybrid stack, which is usually the FR-4 core or the prepreg, not the RF laminate.
  • Connector and shield attach put mechanical load on a thin RF layer. The panel has to leave enough material around SMA and board-edge parts, and depanel is done before the shield is pressed where possible.
  • Rework is possible but limited. The laminate tolerates the temperature; the risk is pad lift on a 3 mil trace. Any rework on an RF trace goes back through impedance verification, not just visual inspection.

Where the unit is exposed to humidity or condensing atmospheres, conformal coating is applied after test. On RF boards the coating changes the effective Dk at the surface, so the impedance target has to account for it at design stage rather than after coating.

Cost: where the premium actually goes

RO4003C material typically costs more than RO4350B, and the gap widens on small panels because material waste is a larger share of the bare-board price. The assembly cost is unchanged. On a hybrid stack, the premium applies only to the RF layers, so a six-layer board with two RO4003C layers carries a much smaller increase than an all-RO4003C construction of the same size.

This is why we quote hybrid and full-RF options side by side. On many programmes the hybrid version delivers most of the loss improvement at a fraction of the cost increase, and the customer can see the trade rather than take it on trust. The cost breakdown page explains which inputs move the number, and the assembly cost calculator gives a budgetary figure for the assembly side before files are final.

Documentation for qualification

RF programmes usually need more paper than digital ones. We supply the laminate lot number against the panel, the impedance report, the micro-section where specified, and the first-article inspection record. For customers running their own qualification, the material certificates come from the laminate manufacturer rather than from us — a distinction worth stating, because a certificate of conformity from the fabricator is not the same document.

The quality assurance page sets out the inspection gates, and the IPC-A-610 acceptance class is agreed before the first lot. Kilandu holds IATF 16949:2016 (0596984), ISO 9001:2015 (CN27125Q0392R0S), ISO 13485:2016 (35825MDQMS0021R0S) and ISO 14001:2015 (CN27125E0142R0S), with UL file E352816.

Frequently asked

Can RO4003C replace RO4350B without a redesign?

Usually yes, with a width adjustment of about 1.5 % to hold impedance. Phase-critical networks need re-checking because electrical length also shifts by roughly 1.5 %.

Is RO4003C suitable above 30 GHz?

It is usable, but RO3003 or RT/duroid 5880 are the more common choices at millimetre-wave frequencies because the loss difference becomes decisive over realistic trace lengths. We build all three and would normally quote them together.

Do you stock RO4003C?

Availability varies by thickness and panel size. Small quantities are usually sourced per order, which affects lead time more than price. The MOQ and lead time page explains the variables.

Can we consign the laminate?

Yes. Consigned material is recorded on the traveller, and the Dk risk moves to the customer's incoming inspection. The sourcing page covers how we handle both routes.

Why build it here

Bare board and assembly under one quality system means a stack-up or impedance problem surfaces at fabrication rather than after the parts are already populated. RF work is quoted by an engineer against the actual stack, and the impedance report ships with the boards. The RF PCB and special board pages cover the adjacent materials, the RF assembly page covers boards with connectors and shields, and the reasons customers stay are set out separately.

Send the stack-up and the loss budget. We will tell you whether RO4003C is needed, quote the hybrid and full-RF options, and state the impedance report format up front.